Table 1. Manufacturing condition of lacquer with woodceramic powder

Manufacturing condition Resin content of woodceramics (%) Carbonization temperature of woodceramics (°C) Addition amount of woodceramics (%)
Lacquer mixed woodceramic powder according to the resin content 40506070 600 10
Lacquer mixed woodceramic powder according to the carbonization temperature 50 6008001001,200 10
Lacquer mixed woodceramic powder according to the addition amount of ceramics 50 600 5101520