Table 1. Composition of prepared composite samples
No. | Conditions | Ratio (%) | Density (kg/m3) | Porosity (%) | Thickness swelling (%) |
Bagasse | CS |
1 | SB100-A | 100 | - | 380 | 189.07 | 2.52 |
2 | SB100-B | 100 | - | 450 | 124.68 | 2.11 |
3 | SB100-C | 100 | - | 520 | 57.42 | 1.35 |
4 | SB75-CS25-A | 75 | 25 | 380 | 123.16 | 0.83 |
5 | SB75-CS25-B | 75 | 25 | 450 | 76.54 | 0.60 |
6 | SB75-CS25-C | 75 | 25 | 520 | 46.50 | 0.37 |
7 | SB50-CS50-A | 50 | 50 | 380 | 111.27 | 0.33 |
8 | SB50-CS50-B | 50 | 50 | 450 | 67.26 | 0.18 |
9 | SB50-CS50-C | 50 | 50 | 520 | 30.54 | 0.08 |
The thickness of the composites was standardized at 30 mm.
CS: coffee silver skin, SB: sugarcane bagasse.