Table 3.
Flame retardancy of plywood treated with difference additives

Sample Remaining flame time (sec) Smoldering time (sec) Carbonized area (mm2) Carbonized length (mm)
less than 10 sec less than 30 sec less than 5,000 mm2 less than 200 mm
F 0 0 7,863 149
G 0 0 5,127 133
H 0 0 3,947 93
I 0 0 2,280 71
J 0 0 2,994 78
K 0 0 4,569 102
L 0 0 4,766 115
M 0 0 7,570 146
N 0 0 8,318 158