Table 1.
Types of test for mechanical properties of acetylated MDF
| Conditions | Mechanical properties |
| Bending strength | Internal bond | Screw holding |
| Air dry | ○ | ○ | ○ |
| Wet treatment | A-testa) | ○ | ○ | ○ |
| B-testb) | ○ | ○ | ○ |
Soaking for 2 hours in hot water at 70±3°C, followed by 1 hour in cold water
Soaking for 2 hours in boiling water, followed by 1 hour in cold water.